Jinhu Color Powder Coating Co.Ltd 86-25-83318869 manager@colorpowdercoating.com
Light Fixture Thermoset Powder Coating Antique Copper Appearance CE Standard

Light Fixture Thermoset Powder Coating Antique Copper Appearance CE Standard

  • High Light

    fluidized bed powder coating

    ,

    automotive powder coating

  • Color
    Pastel Yellow
  • RAL
    R1034
  • Gloss
    70%
  • Appearance
    Antique Copper
  • Impact
    50kg
  • Salt Resistant
    1000Hours
  • Place of Origin
    Ukraine
  • Brand Name
    TOPO
  • Certification
    CE, SGS, BV, ISO
  • Model Number
    TPC-RAL1034
  • Minimum Order Quantity
    Negotiable
  • Price
    Negotiable
  • Packaging Details
    Two-ply PVC bag inside with carton box
  • Delivery Time
    7 days
  • Payment Terms
    Western Union, MoneyGram, L/C, T/T
  • Supply Ability
    400ton/Month

Light Fixture Thermoset Powder Coating Antique Copper Appearance CE Standard

RAL1034 Pastel yellow electrostatic thermoset powder coating for Light Fixtures

 

Antioxidant—A compound that reduces polymeric degradation caused by heat. The thermal degradation of a polymer can cause discoloration (typically yellowing) and a reduction in coating durability and mechanical performance. Antioxidants can be primary or secondary. Primary antioxidants can be used alone or with secondary antioxidants.

 

Binder—The resinous component of a powder formula that provides the film-formation of the coating. The binder is comprised of the resin, crosslinker and binder additives such as catalyst, flow agent, and degassing agent.

 

Catalyst—A compound that increases the rate of a chemical reaction without being consumed by the chemical reaction. Also described as an accelerator. Catalysts are used to lower the cure temperature and/or cure time of a thermosetting powder coating.

 

Colorant Pigment—A material comprised of insoluble particles that provide color and opacity. Pigments produce color by inherently absorbing certain wavelengths of visible light (ranging from approximately 380 to 730 nanometers). This absorption is observed then processed by the human eye and is interpreted by what humans describe as color.

 

Crosslinker—A relatively low molecular weight oligomer possessing two or more chemical groups capable of reaction with thermosetting polymers. Crosslinker is synonymous with “curing agent” and hardener.

 

 

Physical Properties

 

        TP-1 TP-2
Flexibility BS3900 E1 Pass mm 6 5
Scratch BS3900 E2 Pass kg 4 4
Impact BS1391        
  Direct Pass in lbs 80 100
  Reverse Pass in lbs 80 100
Erichsen Cupping BS3900 E4 Pass mm 6 8
Cross Hatch BS3900 E6 Pass % 100 10

 

 

Suit your widest needs

  • Household appliances.

  • Automotive parts.

  • Bicycle components.

  • Coating of aluminum extrusions.

  • Window trims.

  • Wind powers.

  • Agricultural equipment.

  • Aerospace areas.

  • Interior and exterior furniture.

  • Architecture construction.

  • Metal fence and rails.

  • Goods display, etc.

 

Testing Items Standard Data
Appearance   Flat And Smooth
Coating Thickness GB/T6554-2003 50~70mm
Gloss(60°) GB/T9754-2007 From 2%~100% to All Gloss
Impact Resistance GB/T1732-1993 50kg.cm
Bending Performance GB/T6742-2007 2mm
Cupping  GB/T9753-2007 8mm
Adhesion Force GB/T9286-1998 0 Grade
Hardness GB/T6739-2006 2H

Resistant to Salt 

(1000 Hours)

GB/T1771-2007 No Change For Coating Appearance
Humidity And Heat Resistance (1000 Hours) GB/T1740-2007 No Change For Coating Appearance

Chemical Medium Resistance (240 Hours)

5%H2SO4

5%HCl

5%NaOH

5%NaCl

GB/T1763-1979

 

 

No Change For Coating Appearance

No Change For Coating Appearance

No Change For Coating Appearance

No Change For Coating Appearance

Heat Resistance GB/T1735-2009 It Can Reach Between 220℃/20minutes And 240℃/40minutes According To Color And Different Requirement

 

      

                  Light Fixture Thermoset Powder Coating Antique Copper Appearance CE Standard 0   Light Fixture Thermoset Powder Coating Antique Copper Appearance CE Standard 1